Item | Teknologi | Aliran | Kapadhetan | Kekerasan | Ukuran | Isi | Aplikasi |
HRNi20A | Gas Atomized | 12-17s / 50g | 3,5-4,5 g/cm3 | 18-22HRC | -106+45um -90+45um | C:0.1 Kr:4.5 Si: 2.0 B:0.7 Ni: bal. | Semprotan api / fusing, Cetakan kaca, macem-macem dies casting. |
HRNi22A | Gas Atomized | 12-17s / 50g | 3,5-4,5 g/cm3 | 20-24HRC | -106+45um -90+45um | C:0.2 Kr:1.0 Si:2.8 B:1.4 Fe: 1.0 Mn: 0.1 Ni: bal. | Semprotan api/fusing Cetakan kaca, macem-macem dies casting. |
HRNi25 | Gas Atomized | 12-17s / 50g | 3,5-4,5 g/cm3 | 22-27 HRC | -106+45um -90+45um | C:0.2 Kr:1.0 Si: 3.5 B:1.5 Fe: 8.0 Ni: bal. | Semprotan api/fusing Cetakan kaca, macem-macem dies casting. |
HRNi28A | Gas Atomized | 12-17s / 50g | 3,5-4,5 g/cm3 | 26-30HRC | -106+45um -90+45um | C:0.1 Kr:3.0 Si:2.6 B: 1.0 Ni: bal. | Semprotan api/fusing Cetakan kaca, macem-macem dies casting. |
HRNi35 | Gas Atomized | 12-17s / 50g | 3,5-4,5 g/cm3 | 32-37HRC | -106+45um -90+45um | C:0.3 Kr: 10 Si: 3.5 Fe: 10 B:2.0 Ni: bal. | Semprotan api/fusing Cetakan kaca, macem-macem dies casting. |
HRNi37A | Gas Atomized | 12-17s / 50g | 3,5-4,5 g/cm3 | 35-40HRC | -106+45um -90+45um | C:0.15 Kr:4.5 Si:2.6 B:1.2 Ni: bal. | Semprotan api/fusing Cetakan kaca, macem-macem dies casting. |
HRNi45A | Water atomized | 17-21s / 50g | 3,5-4,5 g/cm3 | 42-47HRC | -106+45um -90+45um | C:0.4 Si:3 B:2.6 Kr: 12 Fe: 5 Ni: bal. | Semprotan api / fusing HVOF, permukaan segel, pukulan, katup, piston lsp. |
HRNi50A | Water atomized | 17-21s / 50g | 3,5-4,5 g/cm3 | 45-50HRC | -106+45um -90+45um | C:0.5 Si: 3.0 B:3.0 Kr: 12 Fe: 5 Ni: bal. | Semprotan api / fusing HVOF, permukaan segel, plunger minyak lan poros lsp. |
HRNi55A | Water atomized | 17-21s / 50g | 3,5-4,5 g/cm3 | 52-55HRC | -106+45um -90+45um | C:0.8 Si: 4.0 B:3.0 Kr: 14 Fe: 5.0 Ni: bal. | Semprotan geni / fusingHVOF, permukaan segel, plunger minyak lan poros lsp. |
HRNi60A | Water atomized Gas atomized | 17-21s / 50g | 3,5-4,5 g/cm3 | 55-60HRC | -106+45um -90+45um | C:0.9 Si: 4.0 B:3.2 Kr: 16 Fe: 5.0 Ni: bal. | Semprotan api / fusing HVOF, tahan korosi sing apik, kekerasan dhuwur, kinerja tahan nyandhang sing apik, koefisien gesekan sing sithik. |
HRNi60CuMo | Water atomized Gas atomized | 17-21s / 50g | 3,5-4,5 g/cm3 | 55-60HRC | -106+45um -90+45um | C:0.9 Si: 4.0 B:4.0 Kr: 16 Cu: 3.0 Mo:3.0 Fe: 5.0 Ni: bal. | Semprotan nyala / fusing HVOF, fix, impeller, piston, katup lsp. |
HRNi65A | Water atomized | 17-21s / 50g | 3,5-4,5 g/cm3 | 60-65HRC | -106+45um -90+45um | C:1.1 Si: 4.0 B:4.0 Kr:18 Fe: 5.0 Ni: bal. | Semprotan api / fusingHVOF, kekerasan sing luwih dhuwur tinimbang Ni60A, roller kawat, plunger, roller conveyor dll. |
HRNI625 | Water atomized Gas atomized | 17-21s / 50g | 3,5-4,5 g/cm3 | 8-15HRC | -106+45um -90+45um -45+15um | C:0.1 Si: 0,5 B:0.5 Kr:21 Mo:8.5 Nb: 4.0 Fe: 5.0 Mn: 0.5 Ni: bal. | Semprotan geni / fusing HVOF, istirahat karat sing apik lan kinerja oksidasi suhu anti-dhuwur, |
PS: Kita uga nawakake layanan khusus |
1. Panutup lapisan khusus ing bagean wesi lan baja lan sawetara ndandani cetakan kaca.
2.Pre-proteksi lan ndandani utawa nguatake bagean merchannical.
3. Kanggo aplikasi FLS / PTA / APS / Laser Cladding kanthi campuran lapisan bubuk campuran Ni utawa Nikel.
4.Generate lapisan luwih kandhel dibandhingake karo FTC, lan karo atose luwih apik lan wearness.